item | Test Method | The represent value | |||
Thickness(micro) | ASTM-D374 | 12 micro | 15 micro | 19 micro | 25 micro |
Specific Gravity g/cm3 | ASTM-D1505 | 0.92 | 0.92 | 0.92 | 0.92 |
Contraction rate Lengthwas/horizontal | ASTM-D2732 | 52/54 | 52/53 | 52/53 | 51/52 |
Fog Degree % | ASTM-D1003 | 1.4 | 1.7 | 2.2 | 2.3 |
Clarity degree % | ASTM-D2457 | 125 | 125 | 125 | 120 |
Coefficent of friction | ASTM-D1894 | 0.23 | 0.21 | 0.21 | 0.21 |
Unit area m2/kg | 91 | 72.8 | 57.4 | 43.7 | |
Tensile strength lengthways/Horizontal N/mm2 | ASTM-D883 | 125/120 | 120/125 | 120/110 | 120/110 |
Elongation rate of breaking % lengthways/horizontal | ASTM-D884 | 105/100 | 105/100 | 110/105 | 110/120 |
Tearing-resisting strength(g) | ASTM-D1992 | 6.2 | 10 | 14.5 | 17 |
Heat intensity N/mm2 | Int meth | 40 | 40 | 39 | 39 |
Property | Unit | Value | |||
DENSITY | g/cm3 | 0.92 | |||
THICKNESS | micro | 12.5 | 15 | 19 | 25 |
YIELD | m2/kg | 88.8 | 72.5 | 57.2 | 43.5 |
FLAT WIDTH | m | 3000 | 2500 | 2100 | 1600 |
CENTER FOLD | m | 1500 | 1250 | 1100 | 800 |
SEAL STRENGTH | gr/cm | 1100 | 1100 | 1280 | 1420 |
RESISTANCE | gr | 4/10 | 6/11 | 8/13 | 12/20 |
HAZE | % | 2 | 2.2 | 3.2 | 4 |
GLOSS | PHOTOM | 125 |
Ansprechpartner : | Susan Liao |
---|